Leave Your Message

New Technical Progress: Industrial‑Scale Application of Characteristic Regulation Technology for Nano‑scale, Micro‑scale and Macro Inclusions in High‑Quality Steel

2026-09-07

China maintains an annual crude steel output of around 1 billion tonnes, accounting for over 50 % of global production. Nevertheless, part of domestic high‑grade steels still lag behind world‑class benchmarks in performance stability, restricting the development of key equipment for national economy and defence industries.

Non‑metallic inclusions are critical factors deteriorating steel quality. They trigger surface defects on cold‑rolled sheets, degrade heat‑affected‑zone performance for high‑heat‑input welding heavy plates, abnormal grain growth in gear steels, inspection defects in seamless pipes and line‑pipe steels, as well as deteriorated hot ductility of medium‑high manganese steels.

Modern steelmaking has well‑established impurity‑removal purification processes. However, precise control of multi‑size inclusions remains a major bottleneck for high‑quality steel production. Larger inclusions cause more severe property degradation. Three main technical obstacles exist: nano‑precipitates tend to re‑dissolve at high temperature with unstable functions; diverse micro‑inclusions make multi‑objective coordination difficult; macro inclusions stem from slag entrapment, ladle slag carry‑over, refractory erosion and re‑oxidation across multiple metallurgical steps, making ultra‑cleanliness hard to realise.

Led by Professor Yang Jian from Shanghai University and supported by national R&D programmes, the research team cooperated with major steel producers including Baosteel, Shagang, Shougang Jingtang, Xingcheng Special Steel and Hengyang Valin Steel Tube. A complete set of characteristic regulation technologies targeting nano‑scale, micro‑scale and macro inclusions has been developed for mass‑production of premium steel grades.

Key Innovations

  1. Regulation of Nano‑scale Precipitates

Mg/Ca deoxidation processes combined with Ti/N ratio and melt oxygen potential control promote refined and increased nano‑TiN precipitates. For Mg‑treated steel, number density of TiN particles rises by more than 10 times while average size drops by 40 %. HAZ grain size reduces from 452 μm to 61 μm. Under 500 kJ/cm high‑heat‑input welding, HAZ impact energy at ‑20 °C increases from 31 J to 181 J.

For Nb‑B microalloyed heavy plates, reducing niobium content improves thermal stability of (Ti,Nb)N precipitates. Boron segregation at grain boundaries raises intragranular acicular ferrite (IAF) fraction and significantly enhances low‑temperature toughness at ‑40 °C. For gear steel, Nb microalloying plus thermo‑mechanical rolling‑cooling utilises pinning effect of nano Nb(C,N) particles. The stable austenite grain control temperature rises from ≤930 °C to 960‑1000 °C, achieving grain size grade 7.5 at 980 °C.

  1. Regulation of Micro‑scale Inclusions

Composite deoxidation with Mn‑Ti‑Al‑Mg/Ca generates multi‑component complex inclusions to promote IAF formation in weld heat‑affected zones. Under 500 kJ/cm welding, IAF fraction reaches 55.4 % for Mg‑treated steel and 82 % for Ca‑treated steel, delivering remarkable improvement of low‑temperature impact toughness.

The team clarified how micro‑inclusions influence hot ductility of medium‑high manganese steels. Industrial trial of 16 %Mn‑1.5 %Al TWIP steel was completed on Baosteel's 300‑ton converter caster line, supporting serial development of high‑manganese steel products.

  1. Regulation of Macro Inclusions

For high‑surface‑quality cold‑rolled automotive sheets, large‑sample electrolysis is adopted to characterise scarce macro inclusions. Optimisation of tundish flux, ladle slag carry‑over control, dynamic slag reconditioning and high‑basicity mould flux suppress macro‑inclusion defects on transfer slabs.

Root‑cause analysis identifies CaO‑Al₂O₃‑SiO₂ composite macro inclusions as the source of internal linear defects in seamless tubes. Optimised refining‑continuous casting workflows cut customer complaint rate from 7 cases per ten‑thousand tons down to ≤1 case per ten‑thousand tons. The incidence of "flake defects" drops from 0.50 % to below 0.20 %.

For extra‑wide thin‑gauge line‑pipe steel, optimised SEN geometry and mould flow‑field control mitigate slag entrapment, lifting ultrasonic testing pass rate of slab edges to 99.2 %.

Industrial Application & Benefits

The technologies have been widely implemented at leading domestic steel mills.

Source: Shanghai University