EQUIVALENT STEEL GRADES LIST IN DIFFERENT REGIONS
China (CN) |
Russia (RUS) ГOCT |
Japan (JPN) JIS |
European Union (EU) EN |
United States (US) |
0Cr17Ni4Cu4Nb |
17-4PH / X17CrNi16-4 |
SUS630 |
1.4542 |
AISI 630 / UNS S17400 |
0Cr15Ni5Cu4Nb |
15-5PH /X5CrNiCuSi13-4 |
SUS155 |
1.4545 |
XM-12/ S15500 |
13Cr11Ni2W2MoV |
13Х11Н2В2МФ |
|
|
AISI 961 |
9Cr18 |
95X18 |
|
|
|
18Cr2Ni4WA |
18X2H4BA- |
- |
|
- |
40CrNiMoA |
40X2H2MA |
SNCM240 |
1.6510 |
AISI 8640 |
Cr12MoV |
X12MΦ |
SKD11 |
1.2601 |
AISI D4 |
4Cr5MoSiV1 |
4Х5МФ1С |
SKD61 |
1.2344 |
AISI H13 |
GCr15 |
ⅢX15 |
SUJ2 |
1.3505 |
AISI 5195 |
W6Mo5Cr4V2 |
P6M3 |
SKH51 |
1.3339 |
AISI M2 |
W6Mo5Cr4V2Co5 |
P6M5K5 |
SKH55 |
1.3243 |
AISI M35 |
W2Mo9Cr4VCo8 |
P2M9K8Φ |
SKH59 |
1.3247 |
AISI M42 |
40CrNi2Si2MoVA |
- |
SNCM439- |
1.2767 |
AISI 300M |
GCr15SiMn |
ШХ15СГ |
SUJ3 |
1.3520 |
AISI 5195 |
9Cr18Mo/ 102Cr17Mo |
|
SUS440C |
1.4125 |
AISI 440C |
|
China (CN) GB/T |
Russia (RUS) ГOCT |
Japan (JPN) JIS |
European Union (EU) EN |
United States (US) ASTM |
|
40Mn2 |
35Γ2 |
SMn443 |
AISI 1340 |
|
|
20Cr |
20X |
SCr420 |
AISI 5120 |
|
|
40Cr |
40X |
SCr440 |
1.7035 |
AISI 5140 |
|
38CrSi |
38XC |
|||
|
12CrMo |
12XM |
1.7355 |
||
|
15CrMo |
15XM |
SCM415 |
1.7243 |
AISI 4118 |
|
20CrMo |
20XM |
SCM420 |
1.7321 |
AISI 4120 |
|
35CrMo |
35XM |
SCM435 |
1.7220 |
AISI 4135 |
|
42CrMo |
38XM |
SCM440 |
1.7225 |
AISI 4142 |
|
12CrMo |
12XM |
1.7335 |
||
|
12Cr1Mov |
12X1MΦ |
|||
|
25Cr2MoV |
25X1MΦ |
1.8519 |
||
|
25Cr2Mo1v |
25X1M1ΦA |
1.8572 |
||
|
38CrMoAL |
38X1M1OA |
SACM645 |
1.8509 |
AISI E7140 |
|
50Cr |
50X |
AISI 5150 |
||
|
15CrMn |
18XΓ |
1.7131 |
AISI 5115 |
|
|
20CrMn |
18XΓ |
SMnC420 |
1.7147 |
AISI 5120 |
|
50CrV |
50XΦA |
SUP10 |
1.8159 |
AISI 6150 |
|
30CrMnSi |
30XΓCA |
|||
|
35CrMnSi |
35XΓCA |
|||
|
20CrMnTi |
20XIT |
|||
|
30CrMnTi |
30XIT |
|||
|
12CrNi3 |
12XH3A |
SNC815 |
1.5752 |
AISI E3310 |
|
20CrNi3 |
20XH3A |
SNC620 |
1.6660 |
|
|
20Cr2Ni4 |
20X2H4A |
|||
|
20CrNiMo |
20XH2MA |
SNCM220 |
1.6523 |
AISI 8620 |
|
40CrNiMo |
40XH2MA |
SNCM240 |
1.6510 |
AISI 8640 |
|
40CrNi2Mo |
40XH2MA |
SNCM439 |
1.6563 |
AISI 4340 |
|
45CrNiMov |
45XH2MΦA |
SNCM447 |
1.6563 |
AISI 4340 |
|
18Cr2Ni4WA |
18X2H4BA |
|
China (CN) GB/T |
Russia (RUS) ГOCT |
Japan (JPN) JIS |
European Union (EU) EN |
United States (US) ASTM |
|
9SiCr |
9XC |
|||
|
9Cr2 |
9X1 |
AISI L2 |
||
|
5Cr2W2Si |
||||
|
Cr12 |
X12 |
SKD1 |
1.2080 |
AISI D3 |
|
Cr12Mo1V1 |
X12M1Φ1 |
SKD10 |
1.2379 |
AISI D2 |
|
9Cr2V |
9X2Φ |
AISI L2 |
||
|
CrWMn |
XBΓ |
SKS31 |
AISI O7 |
|
|
9CrWMn |
9XBΓ |
SKS3 |
1.2825 |
AISI O1 |
|
7CrSiMnMoV |
||||
|
5CrMnMo |
5XΓM |
|||
|
5CrNiMo |
5XHM |
AISI L6 |
||
|
3Cr2W8V |
3XB8Φ |
SKD5 |
1.2581 |
AISI H21 |
|
4Cr5MoSiV |
4X5MΦC |
SKD6 |
1.2343 |
AISI H11 |
|
4Cr5MoSiV1 |
4X5MΦ1C |
SKD61 |
1.2344 |
AISI H13 |
|
China (CN) GB/T |
Russia (RUS) ГOCT |
Japan (JPN) JIS |
European Union (EU) EN |
United States (US) ASTM |
|
12Cr18Ni9 |
12X18H9 |
SUS302 |
1.4325 |
AISI 302 |
|
0Cr18Ni9 |
08X18H10 |
SUS304 |
1.4301 |
AISI 304 |
|
0Cr25Ni20 |
08X23H20 |
SUS310S |
1.4951 |
AISI 310S |
|
0Cr17Ni12Mo2 |
SUS316 |
1.4401 |
AISI 316 |
|
|
022Cr17Ni12Mo2 |
03X17H14M2 |
SUS316L |
1.4404 |
AISI 316L |
|
06Cr18Ni11Ti |
08X18H10T |
SUS321 |
1.4541 |
AISI 321 |
|
12Cr12 |
SUS403 |
AISI 403 |
||
|
20Cr13 |
20X13 |
SUS420J1 |
1.4021 |
AISI 420 |
|
30Cr13 |
30X13 |
SUS420J2 |
1.4028 |
AISI 420 |
|
40Cr13 |
40X13 |
1.4031 |
||
|
14Cr17Ni2 |
14X17H2 |
SUS431 |
1.4057 |
AISI 431 |
|
95Cr18 |
95X18 |
|||
|
102Cr17Mo |
SUS440C |
1.4125 |
AISI S44025 |
|
|
90Cr18Mov |
1.4112 |
|||
|
13Cr11Ni2W2MoV |
13X11H2B2MΦ |
|||
|
0Cr13Ni8Mo2 |
|
China (CN) GB/T |
Russia (RUS) ГOCT |
Japan (JPN) JIS |
European Union (EU) EN |
United States (US) ASTM |
|
40CrNi2Si2MoVA |
- |
SNCM439- |
1.2767 |
AISI 300M |
|
TM21oA |
||||
|
AISI C200 |
||||
|
AISI C250 |
||||
|
AISI C300 |
||||
|
AISI D6AL |
||||
|
30Si2MnCrMoVE |
AISI D406A |
|||
|
AISI T250 |
|
China (CN) GB/T |
Russia (RUS) ГOCT |
Japan (JPN) JIS |
European Union (EU) EN |
United States (US) ASTM |
|
20# |
20 |
S20C |
1.1152 |
AISI 1020 |
|
45# |
45 |
S45C |
1.1192 |
AISI 1045 |
|
65Mn |
65Γ |
S65C-CSP |
AISI 1572 |





Whatsapp